Causes and Prevention of steel welding crack

Time:[2016-6-4]  Hits:4013

(A) hot cracking

 

Hot cracking refers to crack under high temperatures generated, also known as high-temperature cracking or solidification cracking, usually generated internally welds may sometimes occur in the heat affected zone, manifestations are: longitudinal cracks, transverse cracks, root crack crater cracks and heat-affected zone cracking.

Its causes is due to the existence of the weld puddle segregation during crystallization, and impurities in the low melting point eutectic crystallization process in the form of a liquid layer between the existence of segregation to form a solidified after a lower intensity, welding stress is large enough when , they will be among just solidified liquid layer or near-solid metal opened a crack.

In addition, if the grain boundaries of the base material there is also a low melting point eutectic and impurities, when welding the tensile stress is large enough, it will also be opened. In short, the thermal cracking is the result of metallurgical factors and mechanical factors working together.

 

 


For its causes, and its prevention measures are as follows:

(1) limit the base metal and welding materials (including rod, wire, flux and shielding gas) easily segregation element content and harmful impurities, in particular, should control the sulfur and phosphorus content and lower carbon content, generally used for welding in steel sulfur content should not exceed 0.04 5% phosphorus content should not exceed 0.055%; in addition the carbon content of the steel from the welding performance worse, general weld carbon content of 0.10% or less in control, thermal cracking susceptibility It can be greatly reduced.

(2) to adjust the chemical composition of the weld metal to improve weld, the weld refined grain products to increase its plasticity, or reduce the degree of dispersion of segregation, control the harmful effects of a low melting point eutectic.

(3) using basic electrodes or flux to reduce the weld containing impurities taken to improve the degree of crystallization of segregation.

(4) an appropriate increase in the shape factor of the weld, using multi-pass welding method avoids the centerline segregation prevented centerline cracks.

(5) the use of reasonable welding sequence and direction, a smaller weld lines can be super, overall warm-up and hammering method, fill the crater at Crater other process measures.

 


(B) cold cracking

 

 

Generally refers to the weld cold cracking during cooling down to the martensite transformation temperature of the temperature range (300-200 deg.] C or less) is produced, can occur immediately after welding, it can also occur in a long time after the welding, it is also called delayed cracking.

There are basic conditions for the formation of 3: welded joint formation of hardened tissue; the presence and concentration of hydrogen diffusion; and there is a large welding tensile stress.

 

 


For its causes, and its prevention measures are as follows:

(1) welding specifications and choose the right line can improve the weld heat affected zone and state organizations, such as preheating before welding, the control layer temperature, slow cooling after welding or the like to accelerate the hot hydrogen molecules from escaping.

(2) using basic electrodes or flux to reduce the oxygen content in the weld diffusion.

(3) electrode and flux before use should be strictly in accordance with the requirements for drying (low hydrogen electrodes 300 ℃ ~ 3 50 ℃ incubated lh; acid electrode l 00 ℃ ~ l50 ℃ incubated lh; solder 200 ℃ ~ 250.C insulation 2h), carefully cleaning the groove and the wire, remove oil, dirt, moisture and rust, etc., in order to reduce the source of hydrogen.

(4) post-weld heat treatment in a timely manner. First, an annealing treatment to eliminate stress, so that quenching and tempering to improve their toughness; two: eliminate the hydrogen treatment is carried out, the hydrogen from the weld joint fully escape.

(5) improve the quality of steel, reducing the steel layered inclusions.

(6) can be taken to reduce stress in a variety of welding process measures.

Copyright:佛山市勝邦鋼結構有限公司 Foshan Shengbang Steel Structure Co., Ltd. Record Number:粵ICP備13078463號
主站蜘蛛池模板: 亚洲 中文 欧美 日韩 在线人 | 五月天色婷婷在线 | 国产欧美精品国产国产专区 | 91在线高清视频 | 欧美高清在线观看 | 亚洲欧美综合另类 | 国产日韩一区二区三区在线播放 | 韩国一级毛片完整高清 | 亚洲欧美国产精品专区久久 | 婷婷激情狠狠综合五月 | 国产精品久久1024 | 特黄特级高清免费视频毛片 | 91最懂男人的午夜社区 | 亚洲国产精品欧美日韩一区二区 | 手机看片1204日韩一区二区 | 国产精选自拍 | 麻豆激情| 97性视频| 日本一区二区不卡在线 | 国产日韩免费 | 美日韩精品 | 免费日本黄色 | 呦视频在线一区二区三区 | 一本久久精品一区二区 | 日本中文字幕在线观看视频 | 91精品国产麻豆福利在线 | 久久五月天婷婷 | 青娱乐自拍视频 | 国产精品亚洲专区在线观看 | 另类综合视频 | 国产精品一区二 | 在线麻豆 | 国产黄色小视频网站 | 动漫av在线播放 | 久久国产成人午夜aⅴ影院 久久国产成人精品麻豆 | 亚洲综合网在线观看 | 免费一区在线 | 欧美视频在线观看免费播放 | 国产123 | aⅴ免费在线观看 | 热久久视久久精品18国产 |