Guangzhou Steel remind you: slab steel welding crack control measures

Time:[2015-6-3]  Hits:5349

Guangzhou Steel remind you: slab steel welding crack control measures
 

Guangzhou Steel slab steel member is large, plate thickness, weld deposit large, complex nodes, residual stress, prone to crack, affecting the quality of welding, which is important and difficult project quality control. Production of general measures are:
1, measures to prevent hot cracking
1) Control of the chemical composition of the weld. I.e. to reduce the low-melting eutectic composition readily segregation elements, such as sulfur and phosphorus content in the welding material and the base material is formed. Reduce the carbon content in the steel, can reduce the thermal cracking tendencies; improve Mn content can improve weld thermal cracking performance.
2) control of welding parameters and conditions. Control of welding current and welding speed, so that the aspect ratio of each cross section of the upper part of bead reach 1.1 to 1.2, can improve thermal cracking performance, while controlling the weld pool shape, do not form easily understood in sharp elongated bath a longitudinal weld surface thermal cracks. Preheat reduces tendency to form cracks; reasonable welding sequence can make the most of the weld at the smaller restraint of welding, reducing the tensile stress suffered weld shrinkage, thermal cracking tendency can be reduced.
2, cold cracking prevention measures
1) Before welding procedure qualification test performed to determine the process parameters.
2) preheat prevents cracking, as well as improve the performance of a certain action.
3) manual welding using low hydrogen electrodes alkaline E5Q / E55 type; CO: gas shielded arc welding flux cored wire can be used; a H08MnA submerged arc welding can be used F5021, and in strict accordance with the provisions drying. Drying temperature is 350-450 ℃, after dried at 100-150cC temperature for 1 ~ 2h, put insulation cylinder used with the check.
4) Choose a reasonable weld profile, in strict accordance with the drawings machining parts groove.
5) each side of the weld within the range of 30 ~ 50mm rust and water clean, reducing the source of hydrogen.
6) cracks often occur on the head welds and weld root, so tacking length, welding foot height and spacing should also make corresponding provisions. If you have to locate the weld in the groove proceeds, weld height should be less than 2/3 of the groove depth, the length should be greater than 40mm. If necessary, prior to tack welding is preheated. Before welding, positioning the weld inspection, it must be removed when re-welding cracks. Tack welding length and spacing, should be considered the base material thickness, structure length.
7) To reduce stress and prevent cracking during welding, the assembly should avoid forced assembly.
8) appropriate to increase the current, lower cooling rate, helps prevent the formation of hardened tissue.
9) Control interlayer temperature should be slightly higher preheat temperature.
10) Q345C soldering should be carried out after a slow cooling to slow cooling rate of the weld and heat affected zone and prevent cold cracking, respond promptly weldment insulation, that is immediately after welding weldment is heated to 250 to 350. And use of asbestos and other insulation 2.6h after air cooling can reduce the hydrogen content in the weld and prevent cold cracking, heating methods, with preheat before width.
Although Guangzhou Steel slab steel construction difficult, but as long as proper control measures, the proportion of component cracking will be greatly reduced, the project will significantly improve the quality of weld cracks will be avoided, can effectively control industrial building projects quality.

Copyright:佛山市勝邦鋼結構有限公司 Foshan Shengbang Steel Structure Co., Ltd. Record Number:粵ICP備13078463號
主站蜘蛛池模板: 国产91精品一区二区麻豆亚洲 | 国产一区曰韩二区欧美三区 | 在线观看国产免费高清不卡 | 欧美一区二区在线观看免费网站 | 国产日韩久久久精品影院首页 | 成年美女黄网站色大片图片 | h视频在线观看免费观看 | 日本欧美视频在线观看 | 亚洲欧美日韩精品久久奇米色影视 | 黄色成人毛片 | 久久国产视频精品 | 色视频免费网站 | 国产午夜人做人免费视频中文 | 首尔站在线观看免费韩剧 | 一级毛片一级毛片一级毛片 | 日韩一区二区精品久久高清 | 欧美亚洲国产成人精品 | 91看片入口| 特黄特色大片免费视频播放 | 蜜柚在线观看免费高清 | 国产精品成人免费福利 | 国产精品日韩欧美亚洲另类 | 国产精品欧美一区二区三区 | www.国产网站 | 久久曰视频 | 亚洲综合色播 | 日日操干 | 国产精品久久久久毛片真精品 | 第一福利在线观看 | 精品特级一级毛片免费观看 | 伊人黄网 | 亚洲六月丁香六月婷婷花 | 我不卡手机影院 | 四虎亚洲国产成人久久精品 | 国产乱老熟视频胖女人 | 日韩欧美亚洲每日更新网 | 无限时间看片在线观看 | 美女紧身裤裆看光了下面 | 国产精品免费福利 | 国产三级网站 | 欧美看片|